Forum
General Discussions
Re: ASNT Ethics Violations
Posted by: Madan L Sharma , E-mail: Address, on August 10, 2008 at 08:09 :In Reply to: ASNT Ethics Violations posted by : John Doe , E-mail: Address, on July 19, 2008 at 14:23 :
These defects,may cause some serious failures.If you know, something is wrong, confront and resolve, with concerned ASNT Level III and end user.Finally the end user is going to be in problem, if any accident happens.You have social responsibility also,please act.ASNT is there to make world safe and support, and weed out the bad elements.You can initiate discussion with ASNT too.But first correct the situation for users.With best wishes.
MLS
----------- Start Original Message -----------
: I have a situation where I discovered an ASNT NDT Levle III falsifying NDT results. How can I report him withut getting Project specific. I have undeniable evidence to support this.
: It was not the end useer's fault so I don't want to cause problems for him.
: I gave him and his company ample time to resolve this but they are hoping I will go away apparently. The person accepted NDT data that had bad data in some reports and weld defects in others. He accepted all of them.
------------ End Original Message ------------
- Re: ASNT Ethics Violations Gerald Newell 14:42 Aug-21-2008 (1)
- Re: ASNT Ethics Violations John Doe 15:35 Aug-21-2008 (0)