: Some one got experiance in TOFD with Nickel Chrome Steel. Nickel 20% and Chrome 15%.. i have a job in hand with 30mm thickness; is that possible to do?
------------ End Original Message ------------

Hi mj,
I am a TOFD specialist working over mainly carbon steels. I have tried TOFD application on 18-10 Cr Ni, as everybody knows the metallurgy is very difficult to explain and standardise. Therefore I could not achive a succesfull experimental. However, i have used 1 MHz probes with very low dB, this helps me too much. If you send the details to me via e-mail, Ý will help you.



Follow Ups:



Post a Followup:

Name:
E-Mail:

Subject:

Comments:

Optional Link URL:
Example: "http://www....html". Alternative write "http://www.ndt.net/wshop/attach/filename.htm" if you transfered a filename.htm via FTP
Page Title: is important!
Optional Image URL:
http://www....gif


Attention! Please click the button only once. This may take a moment to process


Forum Technical Discussions Help